Tytuł: Dipole Relaxation in Semiconducting Zn2−xMgxInV3O11 Materials (Where x = 0.0, 0.4, 1.0, 1.6, and 2.0)
Autor: Groń, Tadeusz
Bosacka, Monika
Filipek, Elżbieta
Pawlus, Sebastian
Nowok, Andrzej
Sawicki, Bogdan
Duda, Henryk
Goraus, Jerzy
Słowa kluczowe: electrical properties; dielectric spectroscopy; relaxation processes
Data wydania: 2020
Źródło: Materials, Vol. 13 (2020), Art. No. 2425
Abstrakt: This paper reports on the electrical and broadband dielectric spectroscopy studies of Zn2􀀀xMgxInV3O11 materials (where x = 0.0, 0.4, 1.0, 1.6, 2.0) synthesized using a solid-state reaction method. These studies showed n-type semiconducting properties with activation energies of 0.147–0.52 eV in the temperature range of 250–400 K, symmetric and linear I–V characteristics, both at 300 and 400 K, with a stronger carrier emission for the matrix and much less for the remaining samples, as well as the dipole relaxation, which was the slowest for the sample with x = 0.0 (matrix) and was faster for Mg-doped samples with x > 0.0. The faster the dipole relaxation, the greater the accumulation of electric charge. These e ects were analyzed within a framework of the DC conductivity and the Cole–Cole fit function, including the solid-state density and porosity of the sample. The resistivity vs. temperature dependence was well fitted using the parallel resistor model. Our ab initio calculations also show that the bandgap increased with the Mg content.
URI: http://hdl.handle.net/20.500.12128/15307
DOI: 10.3390/ma13112425
ISSN: 1996-1944
Pojawia się w kolekcji:Artykuły (WNŚiT)

Pliki tej pozycji:
Plik Opis RozmiarFormat 
Gron_Dipole_relaxation_in_semiconducting.pdf3,64 MBAdobe PDFPrzejrzyj / Otwórz
Pokaż pełny rekord


Uznanie Autorstwa 3.0 Polska Creative Commons Creative Commons